In order to observe the effect, three totally different samples of MRE are fabricated by imposing curing current of zero.1 A, zero.3 A and zero.5 A which is equivalent to the magnetic subject of 70 mT, 309 mT, and 345 mT, respectively. All samples consist of 30% silicone rubber and 70% carbonyl iron particles by weight percentages. After observing the morphological pictures by way of SEM, the dynamic performances of those samples, corresponding to storage modulus and loss factor are evaluated and compared as a operate of the magnetic subject intensity or oscillation frequency. It is proven that the pattern cured at 0.5A reveals the highest storage modulus within the frequency area.